MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Polyhydroxybutyrate - Biopolymer PHB
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: PHB and its copolymers with polyhydroxyvalerate (PHV) are melt-processable semi-crystalline thermoplastics made by biological fermentation from renewable carbohydrate feedstocks. They have been described as "the first example of a true thermoplastic from biotechnology" and are also biodegradeable. Although quite stable under everyday conditions they degrade slowly in the body and when composted or in landfill sites. [The HB monomer unit is a normal constituent of human blood.]

Their chemical resistance is somewhat limited as they are attacked by acids and alkalis and dissolve in chlorinated solvents. Rather remarkably, they are optically active polymers with a chiral site in each molecular repeat unit, all of which are in the D- (or R) configuration.

PHB homopolymer is a stiff and rather brittle polymer of high crystallinity, whose mechanical properties are not unlike those of polystyrene, though it is less brittle and more temperature resistant. Hence, copolymers are preferred for general purposes. It is believed that the most likely area for the application of homopolymer is in the medical/biological fields.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPa
Tensile Modulus 3.50 GPa
Izod Impact, Unnotched 0.350 - 0.600 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 °C
 
Descriptive Properties
Chemical Resistance - AlcoholsFair
Chemical Resistance - AlkalisPoor
Chemical Resistance - Dilute AcidsFair
Chemical Resistance - Greases and OilsGood
Resistance to Ultra-VioletFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
Biomer P304 PHB Biodegradable Polymer
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
Biomer P209 PHB Biodegradable Polymer
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

PGOODF218 / 42289

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.