MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes:
  • Available in North America
  • Additive: Heat Stabilizer, Lubricant and UV Stabilizer
  • Features: Good Toughness, Lubricated, Heat Stabilized
  • RoHS Compliant
  • Auto Specifications: GM GMP.PA66.074 Color: Black
  • Form: Pellets
  • Processing Method: Injection Molding
Properties are for dry polymer unless noted.

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.017 - 0.021 cm/cm
@Thickness 3.17 mm
0.017 - 0.021 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength at Break 34.5 MPa5000 psiConditioned; ASTM D638
 51.7 MPa7500 psiASTM D638
Elongation at Break 55 %55 %ASTM D638
 200 %200 %Conditioned; ASTM D638
Flexural Strength 27.6 MPa4000 psiConditioned; ASTM D790
 68.3 MPa9900 psiASTM D790
Flexural Modulus 0.758 GPa110 ksiConditioned; ASTM D790
 1.72 GPa250 ksiASTM D790
Izod Impact, Notched 8.54 J/cm16.0 ft-lb/inASTM D256
 10.1 J/cm19.0 ft-lb/inConditioned; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmConditioned; ASTM D257
 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Constant  3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
ASTM D150
 5.5
@Frequency 100 Hz
5.5
@Frequency 100 Hz
Conditioned; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C78.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 218 °C425 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C155 °FUnannealed; ASTM D648
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Conditioned
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 293 °C530 - 560 °F
Mold Temperature 48.9 - 87.8 °C120 - 190 °F
Drying Temperature 73.9 °C
@Time 7200 - 14400 sec
165 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.18 %<= 0.18 %Suggested Maximum
Back Pressure 0.138 - 0.414 MPa20.0 - 60.0 psi
Screw Speed 40 - 120 rpm40 - 120 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
Ravago Manufacturing Americas Hylon® N1000THLHF2 Nylon 6/6
Ravago Manufacturing Americas Hylon N1033STHLUV2 Nylon 66
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond)

PENTA107b / 142972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.