MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Top Polymer Topolymer® 9210-851 Thermoplastic Vulcanized Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Production Description: Topolymer® 9210-851 is a heat stabilized PP/EPDM based Thermoplastic Vulcanized Elastomer(TPV). This compound is intended for use in a wide range of applications such as gaskets, seals, covers, electronics or other parts where softness and conformity are needed. 9210-851 can be processed using Injection Molding, Extrusion, Blow molding or other melt processing techniques.

Features:

  • Good resistance to ozone and excellent flex fatigue resistance.
  • EU and China RoHS compliant.
  • It is polyolefin based and completely recyclable.
Application: Light colour, easy coloring. Recommended for applications requiring excellent flex fatigue resistance, excellent ozone resistance. Used in interior, encapsulation applications and sealing applications. These grades of Topolymer TPVs can be processed on conventional thermoplastics equipment for injection molding, extrusion or blowmolding.

Information provided by Top Polymer Enterprise

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585
Tensile Strength 15.5 MPa2250 psi
Elongation at Break 510 %510 %
Tear Strength 55.1 kN/m314 pli
Compression Set 43 %
@Temperature 70.0 °C,
Time 79200 sec
43 %
@Temperature 158 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 175 - 190 °C347 - 374 °FInjection
Middle Barrel Temperature 180 - 195 °C356 - 383 °FInjection
Front Barrel Temperature 185 - 200 °C365 - 392 °FInjection
Nozzle Temperature 185 - 210 °C365 - 410 °FInjection
Melt Temperature 190 - 220 °C374 - 428 °FExtrusion
Head Temperature 190 - 220 °C374 - 428 °FExtrusion
Mold Temperature 25.0 - 55.0 °C77.0 - 131 °FInjection
Drying Temperature 80.0 °C176 °FInjection/Extrusion
Dry Time 3.00 hour3.00 hourInjection/Extrusion
Moisture Content <= 0.080 %<= 0.080 %Injection
Back Pressure 0.350 - 0.700 MPa50.8 - 102 psiInjection
Clamp Pressure 40.0 - 70.0 MPa5800 - 10200 psiInjection
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
ColorNatural color or black
Compress Ratio2:1-4:1
Screw L/D16:1-24:1
Suggested Regrind<20%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding
Top Polymer Topolymer® 9210-651 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-751 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-801 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-403 Thermoplastic Vulcanized Elastomer

PTOPO052 / 184564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.