MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Vacfilm® 400Y Vacuum bagging film
Categories: Polymer; Film

Material Notes: Description: Vacuum bagging film. Ideally suited to aerospace and wind energy applications.

Features & Benefits:

  • Tough, high elongation elastomeric film, suitable for de-bulking applications and oven curing of composites up to temperature of 150°C (302°F)
  • Due to the film’s high elasticity, the necessity for pleats is reduced in debulk operations
  • Premium film for wind energy applications
  • Excellent recovery after elongation enables the film to be reused on subsequent debulk operations, making this film one of the most cost effective debulk products in our range
  • Good release from sealant tape

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 microns
 65.0 microns
 75.0 microns
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 360 %ASTM D882
Film Elongation at Break, TD 370 %ASTM D882
Film Tensile Strength at Break, MD 37.0 MPaASTM D882
Film Tensile Strength at Break, TD 40.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
 
Descriptive Properties
ColorYellow
Yield12.74 m2/kg75 µm
 14.71 m2/kg65 µm
 19.12 m2/kg50 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTED313 / 180615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.