MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MRC Polymers NAXELL™ PC110-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Medium Viscosity  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes:
  • Glass content can be varied
  • Can be UV Stabilized
  • Internal and external lubricant can be added
  • Available in Natural and Black - can go colors

Information provided by MRC Polymers Inc.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
nominal; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 11000 psi
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D638
Elongation at Break 8.0 %
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D638
Flexural Strength 16.0 ksi
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D790
Flexural Modulus 500 ksi
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Dart Drop, Total Energy 18.0 ft-lb
@Thickness 3.17 mm,
Temperature 22.8 °C
7.5MPH; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.4 µm/m-°C
@Temperature -40.0 - 35.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 290 °F
@Thickness 3.17 mm
un-annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 280 °F
@Thickness 3.17 mm
un-annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 560 - 620 °F
Middle Barrel Temperature 570 - 620 °F
Front Barrel Temperature 580 - 630 °F
Nozzle Temperature 560 - 630 °F
Melt Temperature 580 - 630 °F
Mold Temperature 150 - 240 °F
Drying Temperature 260 °F
Dry Time 3 - 4 hour
Moisture Content <= 0.020 %
Dew Point <= 0.000 °F
Drying Air Flow Rate 0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 10000 - 20000 psi
Back Pressure 0.000 - 75.0 psi
Cushion 0.250 in
Screw Speed 30 - 75 rpm
 
Descriptive Properties
Fill RateModerate
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MRC Polymers NAXELL™ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity
MRC Polymers NAXELL™ PC23M-20G General Purpose Low Viscosity Polycarbonate 20% Glass Fiber Reinforced
Covestro Makrolon® RW 6265X Polycarbonate, 10% Glass Fiber
Covestro Makrolon® RW 2405 Polycarbonate, 10% Glass Fiber
Covestro Makrolon® EM 9417 Polycarbonate, 10% Glass Fiber

PMRC029 / 89458

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.