MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® OE100-T High Temperature Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Material Description: A two component, high Tg, high temperature grade epoxy designed for semiconductor, underfill, hard-disk drive and hybrid micro-electronics packaging applications. The epoxy can also be used for adhesive and sealing applications in electronics, optical, and medical devices.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccPart B
 1.12 g/ccPart A
Viscosity 45000 - 70000 cP
@Temperature 23.0 °C
50 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
Tensile Modulus 244000 psiStorage
Shear Strength >= 2000 psiLap
 >= 3400 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 3.08
@Frequency 1000 Hz
Dissipation Factor 0.0030
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.0 µm/m-°CBelow Tg
 165 µm/m-°CAbove Tg
Maximum Service Temperature, Air 250 °CContinuous
 350 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 100 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 468 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5657
@Wavelength 589 nm
Transmission, Visible 88 %
@Wavelength 800 nm
Spectral
 >= 94 %
@Wavelength 880 - 1600 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Temperature 150 °C
minimum
 30.0 min
@Temperature 80.0 °C
minimum
Pot Life 180 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorAmberPart B
 WhitePart A
ConsistencyPourable paste
Mix Ratio by Weight10:1
Number of ComponentsTwo
Weight Loss0.38%200°C
 0.5%250°C
 0.84%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP113 Two Component Epoxy
Epoxy Technology EPO-TEK® 375 High Temperature Epoxy
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy
Epoxy Technology EPO-TEK® MA-5 Optical Grade Epoxy
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy

PPOXYT138 / 141177

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.