MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayblend® T90 XG PC/ABS Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC+ABS)-Blend; Vicat/B 120 temperature = 135 °C; easy flowing; optimized surface quality for metallization (steam treatment)

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.20 %ISO 62
Water Absorption at Saturation 0.50 %ISO 62
Viscosity 225000 cP
@Frequency 1000 Hz,
Temperature 260 °C
Melt; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm60x60x2 mm; 260 °C / MT 80 °C; b. o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm60x60x2 mm; 260 °C / MT 80 °C; b. o. ISO 2577
Melt Flow 29.9 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 56.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 61.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50 mm/min; ISO 527-1,-2
Elongation at Yield 5.1 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2400 MPa1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature -30.0 °C
ISO 180-A
 52.0 kJ/m²
@Temperature 23.0 °C
ISO 180-A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180-U
Puncture Energy 51.0 J
@Temperature 23.0 °C
ISO 6603-2
 57.0 J
@Temperature -30.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0025
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 112 °CISO 75-1,-2
Vicat Softening Point 134 °C
@Load 5.10 kg
50°C/h; ISO 306
 135 °C
@Load 5.10 kg
120°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection; ISO 294
Mold Temperature 80.0 °CInjection; ISO 294
Injection Velocity 240 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® W90 XG PC/ABS Blend
Covestro Bayblend® T90 XF PC/ABS Blend
Overview of materials for PC/ABS + Stainless Steel
Covestro Bayblend® T85 HG PC/ABS Blend
Covestro Bayblend® FR3000 PC/ABS Blend

PCOVEST0057 / 201840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.