MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Solef® 1008 PVDF Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes:

Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.

General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystalline thermoplastic which is obtained by polymerizing vinylidene fluoride. Important properties include excellent chemical resistance to most aggressive substances and solvents, excellent mechanical strength and toughness, high abrasion resistance, high temperature capabilities, excellent aging resistance, high purity, resistance to UV and nuclear radiation, excellent intrinsic fire resistance, resistance to weathering, low permeability to most gases and liquids, and easily melt-processed by standard methods of molding and extrusion.

Tensile properties are achieved with varying methods of sample fabrication. Information provided by Solvay Solexis, Inc.

Key Words: Polyvinylidene Fluoride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/ccISO 1183
Water Absorption <= 0.040 %ISO 62 (method 1)
Linear Mold Shrinkage 0.020 - 0.030 cm/cm
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 24 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
@Thickness 2.00 mm
ASTM D2240
Tensile Strength, Ultimate 35.0 - 50.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 53.0 - 57.0 MPa50 mm/min; ASTM D638
Elongation at Break 20 - 50 %50 mm/min; ASTM D638
Elongation at Yield 5.0 - 10 %50 mm/min; ASTM D638
Modulus of Elasticity 2.60 GPa1 mm/min; ASTM D638
Flexural Yield Strength 78.0 MPa2 mm/min; ASTM D790
Flexural Modulus 2.20 GPa2 mm/min; ASTM D790
Izod Impact, Notched 0.550 J/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
Notched V 10 mm; ASTM D256
Coefficient of Friction 0.20 - 0.30ASTM D1894
Coefficient of Friction, Static 0.20 - 0.40ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0 - 10CS10 / 1 kg
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+14 ohm-cmIntensity = 10 mA after 2 min @ 23°C; ASTM D 257; DIN 53483
Surface Resistance >= 1.00e+14 ohmVoltage < 1 V after 2 min - 500 V; ASTM D 257/DIN 53483
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 59.0 J/gCrystallization Heat
 67.0 J/g80°C to end of melting
CTE, linear 120 - 140 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.20 J/g-°C
 1.60 J/g-°C
@Temperature 100 °C
Thermal Conductivity 0.200 W/m-KASTM C177
Melting Point 174 °CCrystallinity by DSC; ASTM D 3418
Crystallization Temperature 140 °C
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
@Thickness 4.00 mm
after annealing 150°C 16 hr; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
@Thickness 4.00 mm
after annealing 150°C 16 hr; ASTM D648
Vicat Softening Point 171 °C
@Load 1.00 kg,
Thickness 4.00 mm
ISO 306
Brittleness Temperature 0.000 - 10.0 °CASTM D746A
Glass Transition Temp, Tg -30.0 °CDMTA
Decomposition Temperature 375 - 400 °CThermal Stability via TGA : beginning - and at 1% weight loss in air
Flammability, UL94 V-0
Oxygen Index 44 %
@Thickness 3.00 mm
sheet; ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Solef® 1010 PVDF Homopolymer
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
Celanese Hytrel® 4056 TPC-ET
Arkema Kynar® 720 Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Arkema KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding

PSOLVS00 / 68417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.