MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Features:

  • Moderate toughness and strength
  • Good stiffness
  • Easy processability
  • Excellent seal properties
  • Applications:

  • Heavy duty shipping sacks requiring moderate toughness and high stiffness
  • Industrial packaging
  • Industrial liners
  • Construction films
  • Automatic packaging film
  • Information provided by Nova Chemicals

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.926 g/ccASTM D792
    Thickness 25.4 microns
     76.2 microns
    Melt Flow 0.80 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Yield 1620 psiMD, 1 mil; ASTM D882
     1770 psiTD, 1 mil; ASTM D882
     1770 psiTD, 3 mil; ASTM D882
     1780 psiMD, 3 mil; ASTM D882
    Elongation at Break 490 %MD, 1 mil; ASTM D638
     630 %MD, 3 mil; ASTM D882
     680 %TD, 3 mil; ASTM D882
     710 %TD, 1 mil; ASTM D882
    Puncture Energy 0.635 JLow Friction Puncture
    Elmendorf Tear Strength MD 295 g1 mil; ASTM D1922
     1080 g3 mil; ASTM D1922
    Elmendorf Tear Strength TD 752 g1 mil; ASTM D1922
     1467 g3 mil; ASTM D1922
    Dart Drop Test 156 g1 mil; ASTM D1709/A
     453 g3 mil; ASTM D1709/A
    Film Tensile Strength at Break, MD 5970 psi3 mil; ASTM D882
     6160 psi1 mil; ASTM D882
    Film Tensile Strength at Break, TD 4800 psi1 mil; ASTM D882
     5100 psi3 mil; ASTM D882
    1% Secant Modulus, MD 33360 psi3 mil; ASTM D882
     33940 psi1 mil; ASTM D882
    1% Secant Modulus, TD 36400 psi1 mil; ASTM D882
     37700 psi3 mil; ASTM D882
     
    Optical PropertiesOriginal ValueComments
    Haze 13.9 %
    @Thickness 0.0254 mm
    ASTM D1003
     16.6 %
    @Thickness 0.0762 mm
    ASTM D1003
    Gloss 50 %1 mil, at 45°; ASTM D2457
     61 %3 mil, at 45°; ASTM D2457
     
    Processing PropertiesOriginal ValueComments
    Melt Temperature 210 - 230 °C

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
    NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin
    NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
    NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin
    NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin

    PNOV924 / 54870

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.