MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos H19G-01 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Grade H19G-01 is a polypropylene homopolymers designed for extrusion processing and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.
    Applications:
  • Continuous Bulked Filament Yarn
  • Continuous Filament Yarn
  • Staple Fiber
    Benefits:
  • Color Stability
  • Consistent Processing
  • Excellent Spinning Characteristics

Key Words: Excellent Spinning Characteristics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.913 g/ccASTM D792
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength at Break 3490 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 5400 psi2.0 in/min; ASTM D638
Elongation at Break 23 %2.0 in/min; ASTM D638
Elongation at Yield 8.9 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 258000 psiASTM D790A
Izod Impact, Notched 0.500 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 1.33 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 226 °FUnannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 79 %
@Thickness 1.27 mm
ASTM D1003
Gloss 95 %60°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessFiber

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H02C-00 Polypropylene Homopolymer
Ineos H35Z-00 Polypropylene Homopolymer
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG
Ineos H11G-01 Polypropylene Homopolymer
Ineos H12E-00 Polypropylene Homopolymer, Antistatic

PINEOS901 / 104594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.