MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

(Viewing data as-entered. Click here to return)
Klinger Thermoseal KLINGERSIL® C-4201 General Application Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Synthetic Fiber
  • Nitrile Binder
  • Excellent Resistance to Oil & Solvents
  • Good Anti-Stick Properties
  • Excellent OEM Material

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccASTM F1315
Thickness 1588 micronsThickness tested
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 14.0 kV/mmASTM D149-95a
 
Descriptive Properties
ColorWhite or Black(Top/Bottom)
Compressibility7 percentASTM F36J
Creep Relaxation20 percent1/32", ASTM F38B
Gas Permeability<0.5 ml/minDIN 3535/6
Klinger Hot Compression Test11 percentInitial, Thickness Decrease 73°F (23°C)
 19.5 percentAdditional, Thickness Decrease 572°F (300°C)
Leachable Chloride Content200 ppmFSA Method (Typical)
Recovery>50 percentASTM F36J
Sealability<0.5 ml/hr1/32", ASTM F37A
Thickness Increase0-5%ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
 0-5%ASTM Oil IRM903, 5h/300°F (149°C)
 0-5%ASTM Fuel A, 5h/73°F (23°C)
 0-5%ASTM Fuel B, 5h/73°F (23°C)
Weight Increase<10%ASTM F146 after immersion in Fuel B 5h/73°F (23°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Klinger Thermoseal ML-N562 PTG Gasketing
Klinger Thermoseal ML-5270 PTG Gasketing
Portland Cement with Treated Silica Fume
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M22 Moldable
Klinger Thermoseal RG-S160 PTG Gasketing

PTHERM905 / 146058

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.