MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Borealis HE4872 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HE4872 is a HDPE compound for solid insulation of symmetric data cable at high extrusion speed. Applications: high frequency data transmission cables, outer skin of foam-skin constructions. Specifications: ISO 1872-PE, KGHN, 45-D006; ASTM D1248 Type III, Class A, Category 4, Grade E8, E9; EN 50290-2-23; IEC 61156; and EN 50288.

Information provided by Borealis AG

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/ccISO 1183/ISO 1872-2
ESCR 10% Igepal® >= 80 hour
@Temperature 50.0 °C
F20; IEC 60811-4-1/B
Oxidative Induction Time (OIT) >= 60 min
@Temperature 200 °C
IEC 60811-4-2/B
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5815s; ISO 868
Tensile Strength at Break 20.0 MPaISO 527
Elongation at Break >= 600 %ISO 527-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmIEC 60093
Dielectric Constant 2.33
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.000070IEC 60250
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 - 120 °Cconductor preheating temperature
Melt Temperature 220 - 250 °C
Die Cooling Temperature 30.0 - 50.0 °Cwater cooling

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HE3366 High Density Polyethylene
LyondellBasell Alathon® M6080WC High Density Polyethylene
BASF Novolen® 3300 MC Polypropylene
BASF Novolen® 2700 L Polypropylene
LyondellBasell Alathon® M5370WC High Density Polyethylene

PBOREA485 / 108744

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.