MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Minlon® 11C40 NC010 PA66-IMD40  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: 40% Mineral Reinforced Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccDAM; ISO 1183
Water Absorption 1.1 %
@Time 86400 sec
DAM; Sim. to ISO 62
 5.8 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 63.0 MPa50% RH; ISO 527-1/-2
 90.0 MPaDAM; ISO 527-1/-2
Elongation at Break 10 %DAM; ISO 527-1/-2
 35 %50% RH; ISO 527-1/-2
Tensile Modulus 2600 MPa50% RH; ISO 527-1/-2
 5900 MPaDAM; ISO 527-1/-2
Flexural Modulus 2000 MPa50% RH; ISO 178
 5400 MPaDAM; ISO 178
Poissons Ratio 0.35DAM; ISO 527-1/-2
 0.3850%RH; ISO 527-1/-2
Izod Impact, Notched (ISO) 100 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1U
 100 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
 150 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 200 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmDAM; IEC 62631-3-1
Dielectric Constant 3.9
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.2
@Frequency 100 Hz
DAM; IEC 62631-2-1
Dielectric Strength 24.0 kV/mmDAM; IEC 60243-1
Dissipation Factor 0.010
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.010
@Frequency 100 Hz
DAM; IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 64.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°CDAM; ISO 11359-1/-2
Melting Point 256 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °CDAM; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.810 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 26 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 - 305 °CInjection
 295 °CInjection Optimum
Mold Temperature 70.0 - 120 °CInjection
 100 °CInjection Optimum
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %Injection
Hold Pressure 50.0 - 100 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging G-value (condensate) (mg)0.1ISO 6452; DAM
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Part Marking CodePA66-IMD40ISO 11469
ProcessingInjection Molding
Regional AvailabilityNorth America
 South and Central America
Resin IdentificationPA66-IMD40ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Minlon® 11C40 BKB086 PA66-IMD40
DuPont Mobility and Materials Minlon® 11C140 NC010 PA66-IMD40
DuPont Mobility and Materials Minlon® 12T NC010 PA66-IMD36
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
DuPont Mobility and Materials Minlon® 11C140 BK086 PA66-IMD40

PDSX5243 / 197883

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.