MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP46HT-1 Epoxy For High Temperature Service
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°F is required. It is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly at elevated temperatures. The cured epoxy produces bonds and seals with high mechanical strength and excellent chemical resistance. EP46HT-1 is an excellent choice as a matrix resin for fiber reinforced, high performance, heat resistant composite structures which are resistant to thermal cycling and chemicals, including water, oil and many organic solvents over an wide temperature range of -100°F to +550°F. The fully cured EP46HT-1 polymer system features a glass transition temperature over 235°C. Adhesion to metals, glass, ceramics, wood, vulcanized rubber and many plastics is excellent. The hardened system is an electrical insulator. Color of Part A is tan, Part B is brown. EP46HT-1 is widely used in aerospace, electronic, electrical, computer, construction, metal working, appliance, automotive and chemical industries

Product Advantages:

  • Convenient mixing: product properties relatively unaffected by small changes in mix ratio
  • Easy application: contact pressure only required for cure, system spreads evenly and smoothly
  • For bonding non-drip application version called EP46HT-1ND2 is recommended
  • Convenient cure schedules, fast elevated temperature cures as required
  • Outstanding heat resistance and thermal stability
  • 100% reactive, does not contain any solvents or diluents, excellent dimensional stability
  • Excellent electrical insulation properties even upon prolonged exposure to hostile environments
Key Features:
  • Glass transition temperature over 235°C
  • Excellent dimensional stability
  • Superior durability, thermal shock resistance
  • Long pot life at room temperature
  • Service temperature range of -100°F to +550°F
  • High bonding strength Information provided by MasterBond®
Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 27000 - 30000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 90
Tensile Strength at Break 10600 psi
Elongation at Break 2.9 %
Tensile Modulus 450000 psi
Compressive Strength >= 2400 psi
Shear Strength >= 2500 psiTensile lap, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
Dielectric Strength 435 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°C
Maximum Service Temperature, Air 550 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 177 - 204 °C
 2.00 - 3.00 hour
@Temperature 121 - 149 °C
Pot Life >= 1440 min100 gram batch
Shelf Life 12.0 Monthin original, unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)100:30by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Hexcel® Redux® 308 Modified epoxy film adhesive
Master Bond EP46HT-2AO Black Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy

PMASTB406 / 149653

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.