MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Cerablanket AC2 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Thermal Ceramics Cerablanket AC2 insulating blanket provides enhanced performance over the acoustical properties of Cerablanket AC1. Cerablanket AC2 has been engineered to combine the benefits of improved acoustical performance with high mechanical strength. This combination enables Cerablanket AC2 to perform in the most demanding applications.

Applications:

  • HRSG Silencers
  • Mufflers
  • Sound Walls

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.640 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.420 kg(f)/cm²
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0800 W/m-KASTM C-201
 0.125 W/m-KASTM C-201
 0.193 W/m-KASTM C-201
 0.285 W/m-KASTM C-201
 0.400 W/m-KASTM C-201
Maximum Service Temperature, Air <= 1177 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 45 - 47 %
Other 0.00 - 1.0 %
SiO2 53 - 55 %
 
Descriptive Properties
Airflow Resistivity (Rayls/m)10000 to 15000
Leachable Chlorides (%)<10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Insulfrax® S Blanket Insulation
Unifrax Fiberfrax® Lo-Con™ Felt
DIAB Divinycell® F 50 Sandwich Core Material
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation
MarkeTech Silica Aerogel

CMORF6035 / 202819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.