MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen 5031 L HDPE, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments and glue sticks, connector housings, garden chairs, etc.

Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/cc
Water Absorption 0.010 %
Moisture Absorption at Equilibrium 0.010 %
Linear Mold Shrinkage, Flow 0.016 cm/cm
Linear Mold Shrinkage, Transverse 0.012 cm/cm
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 8.0 %
Tensile Modulus 1.00 GPa
Tensile Impact Strength 75.0 kJ/m²
Tensile Creep Modulus, 1 hour 440 MPa
Tensile Creep Modulus, 1000 hours 290 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Constant 2.4
@Frequency 100 Hz
 2.4
@Frequency 1e+6 Hz
Dielectric Strength 150 kV/mm
Dissipation Factor 0.00020
@Frequency 100 Hz
 0.00020
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 165 µm/m-°C
@Temperature 20.0 °C
Melting Point 131 °C
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
Vicat Softening Point 74.0 °C
Flammability, UL94 HB
@Thickness 0.400 mm
Oxygen Index 17 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 6031 M HDPE, Injection Molding Grade
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
LyondellBasell Hostalen GD 7255 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 5231 HX HDPE, Impact Grade

PSF067 / 66644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.