MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries, PVDF is also gaining recognition in automotive, building, electronics, food processing, pharmaceutical and battery applications. PVDF 11008/0003 combines excellent chemical resistance, dimensional stability and excellent flame and smoke resistance with a moderate degree of flexibility. (For applications requiring high degrees of flexibility, see our 30000 series copolymers.) PVDF 11008/0003 has set the standard for plenum rating jacketing and tubes, consistently achieving UL 150°C rating in numerous cable constructions and fiber raceway designs.
  • Dyneon PVDF 11008/0003 is a copolymer of VF2 and HFP
  • Improved flexibility over PVDF homopolymers
  • Very low smoke and low flame generation
  • Ideal for applications where high strength and a moderate degree of flexibility are required
  • Ideal for high speed extrusion
  • Excellent weatherability
  • Good chemical resistance
  • Long term use temperatures up to 150°C
  • Processable using most conventional thermoplastic conversion techniques

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³ISO 1183
Water Absorption <= 0.040 %<= 0.040 %24 hr @ 23°C; ISO 62 (method 1)
Melt Index of Compound  8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 24 g/10 min
@Load 5.00 kg,
Temperature 230 °C
24 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.0 MPa7540 psi50mm/min; ASTM D638
Elongation at Break 800 %800 %50mm/min; ASTM D638
Flexural Modulus 1.00 GPa145 ksi2mm/min; ASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm10 mA, after 2 min; ASTM D257
Surface Resistivity per Square >= 1.00e+14 ohm>= 1.00e+14 ohm< 1V after 2 min - 500 V; ASTM D257
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FASTM D3418
Flammability, UL94 V-0V-0
Oxygen Index >= 65 %
@Thickness 3.00 mm
>= 65 %
@Thickness 0.118 in
Sheet; ASTM D2863
 
Descriptive Properties
FormGranules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet
BASF Ultradur® B 6550 L PBT
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride
3M Dyneon™ PVDF 11010/0000 Polyvinylidene Fluoride
Arkema Kynar Flex® 3030-15 PVDF

PDYNE067 / 34875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.