MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toray TOYOLAC™ ABS Resin VX10-X01 ABS/PBT Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: ABS/PBT Alloy, PBT+ABS.

General Toyolac™ Notes: TOYOLAC™ ABS is a versatile thermoplastic consisting of acrylonitrile, butadiene, and styrene and it has unique set of properties combining strength, lightness, and aesthetics. TOYOLAC™ is widely used in both industrial and household goods due to its excellent mechanical, chemical, electrical properties, and superior processability.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm23°C/50% RH; Toray Method
Melt Flow 21 g/10 min
@Load 9.99 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108
@Temperature 23.0 °C
50% RH; ASTM D785
 108
@Temperature 23.0 °C
ISO 2039-2
Tensile Strength 43.0 MPaASTM D638
 45.0 MPa
@Temperature 23.0 °C
ISO 527-1,2
Elongation at Break 50 %ASTM D638
 10 %
@Temperature 23.0 °C
ISO 527-1,2
Flexural Strength 66.0 MPaASTM D790
 68.0 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 1.93 GPaASTM D790
 1.98 GPa
@Temperature 23.0 °C
50% RH; ISO 178
Izod Impact, Notched 69.0 J/m
@Thickness 12.7 mm,
Temperature -30.0 °C
V-notched; ASTM D256
 102 J/m
@Thickness 3.20 mm,
Temperature -30.0 °C
V-notched; ASTM D256
 200 J/m
@Thickness 12.7 mm,
Temperature 23.0 °C
V-notched; ASTM D256
 470 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
V-notched; ASTM D256
Charpy Impact, Notched 45.0 kJ/m²
@Temperature 23.0 °C
V-Notched; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °CISO 75-1,2
 92.0 °CUnannealed; ASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY9244 / 248933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.