MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM UV-770 Light Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 52829-07-9

GOYENCHEMUV-770 is special hindered amine type light stabilizer, it can eliminate macromolecular compound, the free radical caused by sunlight. Meanwhile, GOYENCHEMUV-770 also owns good heat stability, it’s cost-efficient and high effective light stabilizer.

Applications:

  • Polyolefin: GOYENCHEMUV-770 is suitable use for PE, PP, TPO, TPU (extraction forming product), excellent weather resistance, usage amount: 0.2-0.5%
  • Polystyrene resin: Provide excellent light stable effect for ABS, IPS, PS, SAN, ASA…etc. Combined with GOYENCHEMUV-328, have synergism effect. Usage amount: 0.3-0.5%
  • Polyurethane: Provide weather resistance of PU leather. Combined with GOYENCHEMUV-328, have synergism effect. Usage amount: 0.3-0.5%
  • Other macromolecular compounds: such as Polyamides, Polyacetals.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 - 86.0 °C
 
Descriptive Properties
AppearanceWhite crystalline powder or granule
Assayby GLC
Color>97%Color of solution (10g/100ml Toluene) 425nm
Loss on drying<0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN518 / 266826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.