MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions HC XV3450 PVC, Flexible  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Transparent

Material Notes: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is "For foods of high water content only". This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
@Time 10.0 sec
ASTM D2240
Tensile Strength at Break 15.9 MPaType IV, 510 mm/min; ASTM D638
Tensile Stress at Strain 8.27 MPa
@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 360 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -38.3 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Contact, Unspecified Rating
USP Class VI Yes
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
FormsPellets
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesHose
 Tubing

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions HC 2170G Polyvinyl Chloride, Flexible
Colorite Polymers Flexchem 5051-02 Vinyl Compound
Colorite Polymers Flexchem 4051-02 Vinyl Compound
Colorite Polymers 9077 Non-Phthalate 77 Series Vinyl Compound
Colorite Polymers 8577 Non-Phthalate 77 Series Vinyl Compound

PH1PN8193 / 102029

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.