MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Insulcast® RTVS 27 NA Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 27 NA is a low viscosity, general purpose, reversion resistant RTV Silicone Compound. RTVS 27 NA finds use in commercial potting/casting applications. RTVS 27 NA’s one-to-one ratio by weight or volume makes it ideal for dispensing equipment or hand mixing. With the ability to cure rapidly at elevated temperatures, RTVS 27 NA can be processed quickly in production situations.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccUncured. Part A
 1.47 g/ccUncured. Part B
Viscosity 2500 cPPart A; ASTM D1084
 2700 cPMixed, Part A, Part B; ASTM D1084
 3000 cPPart B; ASTM D1084
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D2240
Tensile Strength 500 psiASTM D412
Elongation at Break 135 %ASTM D412
Tear Strength 18.0 pliDie B; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.15
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 450 V/milASTM D149
Dissipation Factor 0.0080
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 220 µm/m-°C
Thermal Conductivity 2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
Shrinkage 0.20 %
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 hour
@Temperature 95.0 °C
option
 12.0 - 16.0 hour
@Temperature 25.0 °C
option
Pot Life 60.0 - 90.0 minPart A, Part B
Shelf Life 6.00 MonthPart A, Part B
 
Descriptive Properties
ColorBuff (Neutral)part B, uncured
 Dark Graypart A, uncured
Mix Ratio by volume1:1Part A: Part B
Mix Ratio by weight1:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9120 / 239630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.