MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even after long term exposure to elevated temperatures. It is designed to meet the requirements of Mil-M-14G, Type MFH. Typical uses are connectors, automotive transmission components, computer parts and brush holders.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/ccASTM D792
Apparent Bulk Density 0.800 g/ccASTM D1895
Water Absorption 0.050 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 90.0 MPaASTM D638
Tensile Modulus 17.2 GPaASTM D638
Flexural Yield Strength 124 MPaASTM D790
Compressive Yield Strength 248 MPaASTM D695
Poissons Ratio 0.32
Shear Modulus 6.52 GPaCalculated
Shear Strength 9100 psiafter 16hrs @ 300°F
 12300 psias molded
Izod Impact, Notched 0.267 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Constant 5.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 14.7 kV/mmStep by step; ASTM D149
 16.7 kV/mmShort Time; ASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.5 µm/m-°C
@Temperature 23.0 - 60.0 °C
Specific Heat Capacity 0.280 BTU/lb-°F
Thermal Conductivity 0.00108 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 150 °C
@Thickness 3.00 mm
UL Temp Index
Deflection Temperature at 1.8 MPa (264 psi) 204 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
 5VA
@Thickness 1.50 mm
 
Descriptive Properties
ColorBlack
Feeding & PreformingGood
FormGranular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade

P90X20b / 130909

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.