MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Ateva® 1070 Ethylene Vinyl Acetate Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: Extrusion and injection molding; also recommended for profile and tubing applications and for microcellular crosslinked foam.

Key Words: profile and tubing applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.931 g/ccASTM D1505, ASTM D1928 Proc A
Vinyl Acetate Content 9.0 %
Melt Flow 2.8 g/10 minASTM D1238 190/2.16
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96ASTM D2240
Hardness, Shore D 43ASTM D2240
Tensile Strength, Ultimate 14.0 MPaASTM D638 Type IV
Elongation at Break 685 %ASTM D638 Type IV
Flexural Modulus, 1% Secant 0.101 GPaASTM D790 Method I
 
Thermal PropertiesOriginal ValueComments
Melting Point 101 °CASTM D3417
Vicat Softening Point 81.0 °CASTM D1525
Brittleness Temperature -85.0 °CASTM D746
 
Descriptive Properties
ProcessExtrusion
 Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1030 Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 1010A Ethylene Vinyl Acetate Copolymer Molding Resin
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
Arkema Evatane® 1350 VN 5 Ethylene Vinyl Acetate
Arkema Evatane® 1010 VN 3 Ethylene Vinyl Acetate

PATEVA07 / 25924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.