MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature.

These sealants are fast curing paste consistency products designed for use where quick initial adhesion build is desired. This allows for movement of the sealed assemblies in a shorter period of time increasing productivity.

Mechanical properties for specimen cured 7 days at 25°C and 50% relative humidity.

Key Performance Properties:

  • Primerless adhesion to many metals and plastics
  • Non-corrosive to most substrates
  • Low odor cure
  • Good confined cure properties
  • One-component product - No mixing required
  • Retain elastomeric properties at temperatures of -60C (-75F) to 204C (400F) for long periods and to 260C (500F) for short periods
  • Room temperature cure
  • Excellent electrical insulation properties
  • Excellent UV, chemical and weather resistance

Applications:

The cure properties of these adhesive sealants make them ideally suited for applications in confined spaces. These paste-consistency silicone sealants can be used in thickness up to 6mm (1/4 in.) for bonding and sealing, joining metals and plastics, and electrical insulation.

For applications requiring sealant thickness greater than 6mm (1/4 in.), GE Silicones one component, addition cure or two component silicone rubber compounds are recommended.

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 24
Tensile Strength, Ultimate 21.0 kg(f)/cm²
Elongation at Break 435 %
Tear Strength 7.10 kg(f)/cm
Peel Strength 40.0 pliLexan Polycarbonate®
 42.0 pliGlass
 45.0 pliPVC
 47.0 pli
 48.0 pliAluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 ohm-cm
Dielectric Constant 2.8
@Frequency 100 Hz
Dielectric Strength 17.0 kV/mm
Dissipation Factor 0.0020
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 300 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.0600 W/m-K
Brittleness Temperature -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 hourThrough
Tack-Free Time 0.25 hour
 
Descriptive Properties
Application rate360 g/min
ColorBlack
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White
Momentive Performance Materials RTV566 Silicone Rubber Compound for Low Outgassing Applications
Momentive Performance Materials RTV6108-D1 Two Part Thermal Cure Adhesive
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent

PGESIL041 / 41032

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.