MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtral™ BNT 013 Performance Polyolefin
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.

Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America

Features:

  • Balanced Stiffness/Toughness
  • Ductile
  • Good Colorability
  • Good Surface Finish
  • High Impact Resistance
  • Low Temperature Impact Resistance
Uses:
  • Automotive Applications
  • Automotive Interior Parts
  • Automotive Interior Trim
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2030 psiISO 527-2/50
Tensile Strength, Yield 2610 psiISO 527-2/50
Elongation at Break 60 %ISO 527-2/50
Elongation at Yield 4.0 %ISO 527-2/50
Tensile Modulus 145000 psiSecant; ISO 527-2/50
Flexural Modulus 138000 psiSecant; ISO 178
Charpy Impact, Notched 4.10 ft-lb/in²
@Temperature -30.0 °C
Complete Break; ISO 179
 6.20 ft-lb/in²
@Temperature 0.000 °C
Complete Break; ISO 179
 12.0 ft-lb/in²
@Temperature 22.8 °C
Partial Break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 117 °FISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers Elix™ HH 3110 ABS Polymer
Arkema LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Dow Elvaloy® HP4051 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin

PEX99351 / 175587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.