MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ThyssenKrupp COR-TEN B Structural Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to plates up to 50 mm in thickness made from COR-TEN B.

Definition: Weathering means that due to its chemical composition the COR-TEN B steel, when utilized unprotected, exhibits increased resistance to atmospheric corrosion compared to unalloyed steels. This is because it forms a protective layer on its surface under the influence of the weather. The layer protecting the surface develops and regenerates continuously when subjected to the influence of the weather. In general the covering layer offers protection against atmospheric corrosion in industrial, urban and country-side climate. In cases of particular air pollution by aggressive agents conventional surface protection is recommended. Coating is absolutely necessary in cases of contact with water for long periods, when permanently exposed to moisture, or if it is to be used in the vicinity of the sea. The susceptibility of paint coats to undercreepage by rust is less in the case of weathering steel than in the case of comparable non-weathering steel.

Application: The steel is used for various types of welded, bolted and riveted constructions e.g. steel frame structures, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions.

Information Provided by Thyssen Krupp

Key Words: S355J2W+N; EN 1.8965
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 470 - 630 MPa
@Thickness 16.0 mm
 470 - 630 MPa
@Thickness 16.0 - 50.0 mm
Tensile Strength, Yield >= 345 MPa
@Thickness 16.0 - 50.0 mm
 >= 355 MPa
@Thickness 16.0 mm
Elongation at Break 20 %
@Thickness 16.0 mm
 20 %
@Thickness 16.0 - 50.0 mm
Charpy Impact 27.0 J
@Thickness 10.0 mm,
Temperature -20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.16 %
Chromium, Cr 0.40 - 0.65 %
Copper, Cu 0.25 - 0.40 %
Iron, Fe 96.5 - 98.2 %As Balance
Manganese, Mn 0.80 - 1.25 %
Nickel, Ni <= 0.40 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.30 - 0.50 %
Sulfur, S <= 0.030 %
Vanadium, V 0.020 - 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ThyssenKrupp COR-TEN A Structural Steel
ASTM A572 Steel, grade 50
ThyssenKrupp PAS 355 Structural Steel for Cold Forming
ASTM A656 Steel, grade 1
Bethlehem Steel ASTM A656 Grade 50 Type 7, 3/16 to 2 in. thick, steel plate

NTHYSS048 / 90368

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.