MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D1192 E (SBS) Liner Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1192 E is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms described:
Kraton D1192 ET - supplied as porous pellets dusted with talc
Kraton D1192 ES - supplied as porous pellets dusted with amorphous silica
Kraton D1192 ESM - supplied as powder dusted with amorphous silica
Kraton D1192 ETM - supplied as powder dusted with talc for the North American market

Region: North America, Europe, Asia Pacific, Japan, and South America

Uses: Kraton D1192 E is used for modification of industrial and paving bitumen. It may also be suitable for use in formulating adhesives, sealants and coatings, and in the modification of polymers.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccISO 2781
Bulk Density 0.400 g/cc0.0145 lb/in³ASTM D 1895 method B
Volatiles <= 0.30 %<= 0.30 %KM 04
Molecular Weight 138000 - 162000 g/mol138000 - 162000 g/molTriblock
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.10 - 0.40 %0.10 - 0.40 %ES, ET; ISO 247
 2.5 - 5.0 %2.5 - 5.0 %ESM; ISO 247
 4.0 - 6.0 %4.0 - 6.0 %ETM; BAM 908
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Time 15.0 sec
70
@Time 0.00417 hour
Measured on compression molded slabs; ASTM D2240
 
Descriptive Properties
ContentAntioxidant>0.16%, KM 08
 Polystyrene28.5-32.5%, KM 03
 Total Extractables<1.0%, KM 05
 Vinyl>35%, KM 03
Triblock Content>90%KM 01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dynasol Calprene® 411 Thermoplastic Rubber SBS Dry
Kraton® D1155 E (SBS) Liner Block Copolymer
Kraton® D2122 DO (SBS) Compound
Kraton® D4158 K (O/E SBS) Radial Copolymer
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer

PKRA9838 / 132737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.