MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HB Fuller EternaBond RoofSeal™ MicroSealant® Tape with UV Stable Backer
Categories: Other Engineering Material

Material Notes: Description: RoofSeal™ is a one-step permanent repair system for virtually all roof types and roof accessories. RoofSeal™ features a UV stable backing and creates a waterproof, moisture and air tight barrier with no additional sealing required. RoofSeal™ remains flexible to temperatures as low as -57°C (-70°F) making it virtually impossible to thermally shock the seam causing a leak. RoofSeal™ bonds to a wide range of surfaces including roof materials such as EPDM, TPO, Hypalon, aluminum, galvanized steel, wood, and fiberglass. Ensure all surfaces are clean, dry, and free of debris prior to installation.

Basic Use: RoofSeal™ is used to seal roof joints (seams) and tears, skylights, etc. Perfect for repairing and restoring roofs on mobile homes and RVs. RoofSeal™ seals to itself so it can be cut and folded around an object.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 4.00 - 38.0 °C
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 700 %ASTM D 882
Peel Strength 5.00 pli180°; ASTM D413
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL066 / 316857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.