MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGO® Antifoam 793 Defoamer
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam 793 is a 100 % active defoamer concentrate based on organo-modified siloxanes. TEGO® Antifoam 793 is water dispersible.

Application: TEGO® Antifoam 793 is particularly suitable as defoamer in aqueous based systems. It is used in a wide range of industrial applications, such as

  • Metalworking fluids (MWF)
  • Textile auxiliaries
  • Surfactant concentrates
TEGO® Antifoam 793 can be formulated into concentrates to produce low foaming fluids. Furthermore, it can be used in the ready-to-use fluid as a tank side defoamer. In the case of MWF, TEGO® Antifoam 793 is used in semi-synthetic fluids and soluble oils if incorporated into the concentrate. As a tank side defoamer, it is suitable for all different types of water-based MWF. In alkaline metal cleaners it can be recommended as tank side defoamer

Properties / Benefits:

  • TEGO® Antifoam 793 provides good foam knock down and hold down properties in a broad range of different aqueous based systems.
  • TEGO® Antifoam 793 is free of silicone oils. Therefore, it has no adverse effect on the finishing process (painting/electro-plating, etc.) of the treated parts.
  • TEGO® Antifoam 793 is highly compatible. This allows for the formulation of highly stable concentrates. It also does not deteriorate the shelf-life of ready-to-use emulsions.
  • TEGO® Antifoam 793 is water dispersible, which allows for easy handling.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Viscosity 700 - 1500 cP700 - 1500 cP
 
Descriptive Properties
Appearanceyellowish, turbid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik TEGO® Antifoam 2280 Emulsion
Evonik TEGO® Antifoam 3062 Antifoam concentrate
Evonik TEGO® Antifoam 5-27 Emulsion

PEVONIL542 / 196746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.