MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® PC 40-UMF Single-Component Urethane Acrylate Conformal Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Loctite Stycast PC 40-UMF provides the following product characteristics:
  • Single component
  • VOC free
  • UV and moisture curable

Cure: Ultraviolet (UV) light activation followed by room temperature moisture cure

Application: Conformal coating

Key Substrates:

  • Variety of metal surfaces
  • Ceramic
  • Glass filled epoxy

Loctite Stycast PC 40-UMF conformal coating is specifically formulated to rapidly gel and immobilize when exposed to UV light and then fully cure when exposed to atmospheric moisture, ensuring optimum performance even in shadowed areas.

Loctite Stycast PC 40-UMF conforms to IPC-CC-830 requirements.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccUncured
Viscosity 250 cPNominal Viscosity
Outgassing - Total Mass Loss <= 0.010 %NASA Outgassing; CVCM
 0.36 %NASA Outgassing; WVR
 0.87 %NASA Outgassing; TML
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.50e+16 ohm-cm
Surface Resistance 3.80e+16 ohm
Dielectric Constant 2.75
@Frequency 1e+6 Hz
Dielectric Strength 420 V/mil
@Thickness 2.64 mm
Dissipation Factor 0.12
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.260 W/m-K
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 48.0 - 72.0 hour
@Temperature 23.0 °C
Secondary Cure: Moisture cure for shadowed areas on a populated board
Shelf Life 6.00 Month
@Temperature 20.0 - 30.0 °C
 
Descriptive Properties
AppearanceClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7957 / 255442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.