MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® H5520 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications
ALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, closures and various food containers.

Regulatory Status
H 5520 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing H 5520 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D1505
Melt Flow 20 g/10 minASTM D1238
Spiral Flow 14.2 inSpiral channel (0.625” insert) with injection pressure of 1000 psi at 440°F.; Equistar
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength at Break 3250 psiASTM D638
Tensile Strength, Yield 4160 psiCrosshead speed - 2"min.; ASTM D638
Elongation at Yield 8.1 %Crosshead speed - 2"min.; ASTM D638
Flexural Modulus, 1% Secant 182500 psiCrosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 151000 psiCrosshead speed - 0.5" min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °CASTM D648
Vicat Softening Point 126 °CASTM D1525
Brittleness Temperature -68.0 °CF50; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M6028 High Density Polyethylene
LyondellBasell Alathon® H5618 High Density Polyethylene
LyondellBasell Alathon® ETP H4745 High Density Polyethylene
AlphaGary PVC 2212/S-110 CLEAR 0003 Polyvinyl Chloride Thermoplastic
ExxonMobil HD 56200 High Density Polyethylene Resin

PEQU0125 / 36554

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.