MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is formulated for high speed injection molding and contains nucleating and release additives.

Borpact SG321MO is designed for thin walled containers, lids and houseware articles requiring flexibility, good contact transparency and high impact strength. Examples include thin wall containers, houseware containers and lids, closures with film hinge, and tubes for cosmetic packaging.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ISO 868
Tensile Strength, Yield 2465 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 15 %At 50 mm/min; ISO 527-2
Tensile Modulus 0.600 GPaAt 1 mm/min; ISO 527-2
Charpy Impact, Notched 2.00 J/cm²ISO 179/1eA
 0.650 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
Instrumented Impact Total Energy 18.0 JTotal Penetration Energy; ISO 6603-2
 30.0 J
@Temperature -20.0 °C
Total Penetration Energy; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °CISO 75-2
Vicat Softening Point 45.0 °C50 N; ISO 306
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 250 °C
Mold Temperature 30.0 - 60.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding
Borealis BorPure™ MB7541 High Density Polyethylene for Injection Molding

PBOREA091 / 27398

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.