MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTANAT® EP-MF 201 Polyisocyanate
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: This product is a solvent free, and ready-to-use crosslinker or self-crosslinking binder. It can be used either as a single binder or in combination with appropriate co-binders. These coatings can be cured at ambient temperature and are suitable for all kinds of substrates. VESTANATR EP-MF 202 is a significantly more flexible version. Benefits:
  • Ambient temperature curing
  • Outstanding scratch resistance
  • Solvent free
  • Ready-to-use 1K clearcoat
  • Self-crosslinking hybrid binder
  • Touch-dry within one hour
  • Excellent chemical resistance

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 200 - 300 cP
 
Processing PropertiesOriginal ValueComments
Dry Time 1.00 hour
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %
 
Descriptive Properties
Color<50Hazen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL335 / 196539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.