Sn992 Pb-Free solder is a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross (in wave soldering) than SAC305 and other Sn/Cu based alloys Features - Produces shiny, smooth solder joints under most soldering conditions
- Low cost - does not contain Ag
- Lower dross formation than other SAC and Sn/Cu-based alloys
- Less copper erosion than SAC305
- Compatible with other Sn/Cu-based alloys - no need to dump the pot
- Optimized for use in solder paste form through the addition of Bi
Physical Properties - Time Above Liquidus: 30 to 90 seconds
Information Provided by Indium Corporation |