MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Stellarchem SV-B65E TPV Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on conventional thermoplastics equipment for injection molding or extrusion, provides the performance of vulcanized rubber with the advantage of low cost thermoplastic processing. It's a soft, EPDM/PP based, completely recyclable & colorable elastomer material. It's formulated to overmold to PP thermoplastics in normal dual injection & extrusion processing.

Information provided by Stellarchem Polymer & Industrial

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Particle Mesh Size 80 - 150 Mesh
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ASTM D2240
Tensile Strength, Ultimate 70.0 kg(f)/cm²ASTM D412
Elongation at Break 430 %ASTM D412
100% Modulus 0.02548 GPa
@Strain 100 %
ASTM D412
Tear Strength 23.0 kg(f)/cmASTM D412
Compression Set 26 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 170 °CMetering Temperature, Extrusion
Rear Barrel Temperature 150 - 160 °CExtrusion
 160 - 190 °CInjection Molding
Middle Barrel Temperature 155 - 165 °CTransition, Extrusion
 170 - 190 °CInjection Molding
Front Barrel Temperature 170 - 180 °CExtrusion
 180 - 200 °CInjection Molding
Nozzle Temperature 190 - 210 °CInjection Molding
Die Temperature 170 - 180 °CExtrusion
Melt Temperature 150 - 180 °CExtrusion
 160 - 200 °CInjection Molding
Mold Temperature 25.0 - 40.0 °CInjection Molding
Injection Pressure 5.00 - 40.0 MPaInjection Molding
Back Pressure 0.500 - 1.00 MPaInjection Molding
Screw Speed 60 - 100 rpmExtrusion
 100 - 200 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL 0162-25 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-28 EPDM TPV-Based Thermoplastic Elastomer
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Shandong Dawn Dawnprene 551B1 TPV (EPDM/PP)
Shandong Dawn Dawnprene 551N1 TPV (EPDM/PP)

PSTELL044 / 108267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.