MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Global EPP PA 66E Extruded Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded

Material Notes: Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecular chains. Their combined strengths and characteristics position them as obvious first choice materials for all components, subject to structural and wear conditions, in mechanical and plant engineering environments.

Key characteristics:

  • Excellent sliding and wear properties
  • Perfect balance of mechanical strength, toughness and rigidity
  • Good electrical insulating properties
  • Various FDA compliant grades available.

    This grade is noted for its elevated mechanical strength, rigidity, abrasion and heat resistance. Its impact strength and vibration damping abilities are reduced when compared to PA 6, making this the preferred extruded grade for highly stressed, thermally loaded components.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.145 g/ccTest Method A; ISO 1183:1987
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
Immersion; ISO 62:1999 (modified)
Moisture Absorption at Equilibrium 2.7 %50% RH; ISO 62:1999
Water Absorption at Saturation 8.5 %ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ISO 868:2003
Tensile Strength at Break 90.0 MPaSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 30 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 3.70 GPaSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 100 MPa1.5 mm/min; ISO 178:2001
Flexural Modulus 3100 MPa1.5 mm/min; ISO 178:2001
Compressive Strength 90.0 MPaSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 3200 MPaSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.70 kJ/m²Sample Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.25
@Pressure 1.75 MPa
31.4 m/min
Limiting Pressure Velocity 0.100 MPa-m/sec
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.3
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 30.5 kV/mmIEC 60243-1:1998-01
Dissipation Factor 0.024
@Frequency 100 Hz
IEC 60250:1969-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Thermal Conductivity 0.230 W/m-KISO 8301:1991
Melting Point 260 °C
Maximum Service Temperature, Air 100 °CContinuous
 170 °CIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75
Glass Transition Temp, Tg 72.0 °CISO 11359-2:1999
Flammability, UL94 HBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorNatural, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polypropylene, Extrusion Grade
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative
M Chemical GUARD DOG™ UV360 Light Absorber
M Chemical GUARD DOG™ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative

PGLOEPP01 / 79512

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.