Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics: - Excellent electrical property
- Excellent temperature resistance, high heat distortion temperature.
- Excellent mechanic and chemical property
- Excellent weatherability
- Excellent wear property
- Excellent moldability
- High resistance to fuels, oil, fats and many solventsInformation provided by Gromax Enterprises Corp.
|