MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® SP-202 Conductive Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Vespel® SP-202 has the combination of capabilities that meet these demanding applications.
  • Electrostatic charge removal. Vespel® SP-202 is a conductive plastic grade with surface and volume resistivity values in the range of 10–1 to 101 (ohm, ohm-cm).
  • Vespel® SP-202 has the thermal resistance to maintain tolerances in high heat applications and through multiple thermal cycles.
  • Lower wear rates on contact surfaces generate longer part life and cleaner environments.
  • Vespel® SP-202 can be machined to tight tolerances with relative ease.
Benefits:
  • Although material cost is higher than some engineering plastics, lower scrap rates and machining cost may yield offsetting savings during the fabrication process.
  • Low wear rates will provide consistent positioning and long part life resulting in high production utility and low maintenance cost.
  • Low particle generation will keep operating environments clean.
  • Properly grounded components will not hold a charge preventing the attraction of dust and other charged particles.

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Water Absorption 0.23 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 51Parallel; ASTM D785
 66Perpendicular; ASTM D785
Tensile Strength at Break 28.0 MPa
@Temperature 260 °C
Parallel; ASTM D638
 53.0 MPa
@Temperature 260 °C
Perpendicular; ASTM D638
 56.0 MPa
@Temperature 22.8 °C
Parallel; ASTM D638
 92.0 MPa
@Temperature 22.8 °C
Perpendicular; ASTM D638
Elongation at Break 2.6 %
@Temperature 22.8 °C
Parallel; ASTM D638
 2.6 %
@Temperature 260 °C
Parallel; ASTM D638
 4.5 %
@Temperature 22.8 °C
Perpendicular; ASTM D638
 5.2 %
@Temperature 260 °C
Perpendicular; ASTM D638
Tensile Modulus 1800 MPa
@Temperature 260 °C
Parallel; ASTM D638
 2600 MPa
@Temperature 260 °C
Perpendicular; ASTM D638
 2800 MPa
@Temperature 22.8 °C
Parallel; ASTM D638
 3700 MPa
@Temperature 22.8 °C
Perpendicular; ASTM D638
Flexural Strength 89.0 MPa
@Temperature 260 °C
Perpendicular; ASTM D790
 91.0 MPa
@Temperature 260 °C
Parallel; ASTM D790
 159 MPa
@Temperature 22.8 °C
Perpendicular; ASTM D790
 164 MPa
@Temperature 22.8 °C
Parallel; ASTM D790
Flexural Modulus 4600 MPa
@Temperature 260 °C
Perpendicular; ASTM D790
 4600 MPa
@Temperature 260 °C
Parallel; ASTM D790
 6300 MPa
@Temperature 22.8 °C
Perpendicular; ASTM D790
 6500 MPa
@Temperature 22.8 °C
Parallel; ASTM D790
Compressive Strain at Break 21 %
@Temperature 260 °C
Parallel; ASTM D695
 26 %
@Temperature 22.8 °C
Parallel; ASTM D695
 27 %
@Temperature 260 °C
Perpendicular; ASTM D695
 30 %
@Temperature 22.8 °C
Perpendicular; ASTM D695
Compressive Strength 105 MPa
@Temperature 260 °C
Perpendicular; ASTM D695
 114 MPa
@Temperature 260 °C
Parallel; ASTM D695
 206 MPa
@Temperature 22.8 °C
Perpendicular; ASTM D695
 230 MPa
@Temperature 22.8 °C
Parallel; ASTM D695
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.10 ohm-cmPerpendicular; ASTM D991
 1.0 ohm-cmParallel; ASTM D991
Surface Resistance 0.10 ohmParallel; ASTM D991
 1.0 ohmPerpendicular; ASTM D991
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°C
@Temperature 35.0 - 300 °C
Perpendicular; ASTM E831
 86.0 µm/m-°C
@Temperature 35.0 - 300 °C
Parallel; ASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® ASB-5760 Carbon Graphite
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Arkema Pebax® 5533 SN 70 BLACK Polyether Block Amide (PEBA) (Dry)
DuPont Mobility and Materials Vespel® CP-0301 Fiber Compound

PDTA2002x / 183710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.