MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren™ LIM 8040 Liquid Silicone Rubber - Healthcare  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding process allows for complex part geometry and exact dimensions. LSR elastomers are generally suitable for short cycle time injection and full automatic flash-less processing. Color pastes are available to pigmenting addition cure productions of LSR's.

All LSR grades are platinum cured materials which are mixed in a 1:1 ratio by weight.

The distinctive properties of silicone elastomers - purity, clarity, strength - coupled with ease of processability, have resulted in their use in a broad range of medical device applications. Silicone materials exhibit exceptional stability over a wide range of temperatures, lending themselves to use in applications requiring repeated sterilization performance.

Typical applications include, but are not limited to:

  • Dental / surgical devices
  • Diagnostics / imaging
  • Fluid and drug delivery devices
  • Orthopedics / prosthetics
  • Scar management
  • Septa / stoppers / laboratory accessories
  • Medical tubing
  • Wound drains and bulbs
  • Sterilization mats
  • Pharmaceutical closures
  • Instrument grips
  • Dialysis o-rings
  • Positioning devices
  • Catheters
  • Seals / o-rings / valves
  • Respiratory / anesthesia
  • Medical equipment keypads

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Linear Mold Shrinkage 0.027 cm/cmvulcanized 10 sec at 200°C; Without post-cure
 0.035 cm/cmvulcanized 10 sec at 200°C then post-cured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 39
Tensile Strength 7.00 MPa
Elongation at Break 640 %
Tear Strength 36.0 kN/mDie B
Compression Set 20 %Post cured
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %transparent; thickness unknown
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 20.0 °Ccool nozzle and cylinder to prevent premature vulcanization
Mold Temperature 140 - 230 °Cshort vulcanization time required (a few seconds)
Injection Pressure 5.00 - 15.0 MPadepends on feed channel
Hold Pressure 5.00 MPa
 
Compliance PropertiesOriginal ValueComments
FDA YesFDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
USP Class VI YesUSP Class VI methods: Intramuscular implantation, intracutaneous injection, & systematic injection
 
Descriptive Properties
AppearanceTransparent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LIM 8040 Liquid Silicone Rubber - Self-Bonding
Momentive Performance Materials Silopren™ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized
Momentive Performance Materials Silopren™ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized
Momentive Performance Materials Silopren™ LSR 2740 Liquid Silicone Rubber - Healthcare
Dow DOWSIL™ MS-4022 Optical Grade Moldable Silicone

PGE8V757 / 109017

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.