MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Chemical Titan TITANPRO® SM488 Polypropylene random copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Titanpro SM488 is a superb clarity grade designed for high transparency articles. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.

TSCA Registry: CAS# 9010-79-1

Applications:

  • Superb clarity ISBM articles, baby bottles, drinking containers, housewares, healthcare devices, thin-walled containers, storage containers
Advantages:
  • Superb clarity
  • Good balance of rigidity and impact resistance
  • Good surface finish and color
  • Suitable for hot filling
Fabrication:
Equipment - injection stretch blow molding (ISBM) machine, injection molding machine
Techniques - standard processing

Information provided by Titan Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.900 g/ccASTM D1505
Water Absorption 0.020 %
@Time 86400 sec
ASTM D570
Base Resin Melt Index 20 g/10 min
@Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 92ASTM D785A
Tensile Strength, Yield 290 kg(f)/cm²ASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus 12000 kg(f)/cm²ASTM D790B
Izod Impact, Notched 6.00 kg-cm/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 5112 C Clarified Random Polypropylene Copolymer, Injection Molding Grade
Bamberger Polymers Bapolan® 6055 Polystyrene, Injection Molding
Lotte Chemical Titan TITANPRO® SM198 Polypropylene random copolymer
Lotte Chemical Titan TITANPRO® SM388 Polypropylene random copolymer

PTITAO08 / 183292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.