MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 3015/70 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 3015/70 A/B liquid silicone rubber is a paste like, readily pigmentable two-component compound with extremely short curing time. Its vulcanizates are noted for their high oil resistance. They are colored off white and have moderate mechanical properties. Thanks to the excellent compression set, there is no need to post-cure technical parts.

Application: ELASTOSIL® LR 3015/70 A/B is particularly suitable for the economical production of large series of injection molded articles. Parts made from ELASTOSIL® LR 3015/70 A/B can generally be used for technical applications without post-curing, but do not comply with regulations concerning use in the pharmaceutical and food industry. Due to their high oil resistance, ELASTOSIL® LR 3015/70 A/B is mainly used to produce gaskets for automotive and other mechanical engineering applications.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccDIN EN ISO 1183-1 A
Viscosity 600000 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 58Oil immersion (70h/150°C),Lubrizol OS 206 304
 59Oil immersion (70h/150°C), IRM 903
 68Oil immersion (70h/150°C), IRM 901
 70DIN 53505
Tensile Strength at Break 4.60 MPaOil immersion (70h/150°C),Lubrizol OS 206 304
 4.80 MPaOil immersion (70h/150°C), IRM 903
 5.80 MPaOil immersion (70h/150°C), IRM 901
 6.00 MPaDIN 53504 S 1
Elongation at Break 220 %Oil immersion (70h/150°C), IRM 903
 220 %Oil immersion (70h/150°C),Lubrizol OS 206 304
 240 %Oil immersion (70h/150°C), IRM 901
 280 %DIN 53504 S 1
Tear Strength 18.0 kN/mASTM 624 B
Compression Set 16 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °Cwith heat stabilizer
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
in press
 
Descriptive Properties
Appearancebeige
Volume Swell (%)15Oil immersion (70h/150°C),Lubrizol OS 206 304
 33Oil immersion (70h/150°C), IRM 903
 4Oil immersion (70h/150°C), IRM 901

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9114 / 204643

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.