MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Greene Tweed CHEMRAZ® 644 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Specifically developed to meet the demands of aggressive dry plasma systems and the corresponding remote O2 cleaning processes, Chemraz® 644, a perfluoroelastomer with a unique formulation, provides enhanced plasma resistance and minimal contamination resulting in less downtime and higher wafer processing yields. Recommended primarily for both static and dynamic oxide etch wafer processing applications, Chemraz 644 remains stable at service temperatures up to 315°C (600°F).

Applications:

  • Endpoint windows
  • Bell jar seals
  • Valve seals
  • KF fitting seals
  • Window seals
  • Isolator valve seals
  • Lid seals
  • Gas inlet seals
  • Slit valves seals
  • Chamber seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.03 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Tensile Strength at Break 1794 psiASTM D1414
Tensile Strength, Yield 326 psi@50% Elongation; ASTM D1414
 633 psi@100% Elongation; ASTM D1414
Elongation at Break 207 %ASTM D1414
Compression Set 25 %
@Temperature 204 °C,
Time 252000 sec
At 25% deflection; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 315 °F
Minimum Service Temperature, Air -4.00 °F
 
Descriptive Properties
ColorDark Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
Greene Tweed CHEMRAZ® 640 Perfluoroelastomer
Greene Tweed CHEMRAZ® 639 Perfluoroelastomer
Greene Tweed CHEMRAZ® 629 Perfluoroelastomer

PGREEN29 / 42323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.