MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa FRABS V-0 Flame Retardant ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes:
    Features:
  • UL 94 V-0 @ 1.5-3.0mm
  • High toughness
  • For extrusion molding

    Applications:
  • Plate
  • Electric and electronic cabinet
  • PCB board

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/cc
@Temperature 23.0 °C
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Temperature 23.0 °C
ASTM D955
Melt Flow 1.2 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 15 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength at Break 40.0 MPa50mm/min; ASTM D638
Elongation at Break 15 %50mm/min; ASTM D638
Flexural Strength 58.0 MPa2mm/min; ASTM D790
Flexural Modulus 2200 MPa2mm/min; ASTM D790
Izod Impact, Notched 143 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 176 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 22.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 93.0 °C
@Load 5.00 kg
50°C/hr; ASTM D1525
 102 °C
@Load 1.00 kg
120°C/hr; ASTM D1525
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 245 °C
Rear Barrel Temperature 180 - 210 °CStart Point: 190°C
Middle Barrel Temperature 190 - 220 °CStart Point: 205°C
Front Barrel Temperature 200 - 230 °CStart Point: 215°C
Melt Temperature 200 - 230 °CStart Point: 220°C
Mold Temperature 30.0 - 60.0 °CStart Point: 50°C
Drying Temperature 70.0 - 80.0 °C
@Time 7200 - 14400 sec
Pre-dry
Back Pressure 0.000 - 1.00 MPa
 
Descriptive Properties
Injection SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS VP-11 ELG
Kingfa FRABS-518 Flame Retardant ABS
Kingfa HF-626 Flame Retardant ABS
Omni Plastics OmniTech™ FRABS ABS
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow

PKINGF109 / 104368

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.