MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis RD208CF Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films on chill roll processes. RD208CF is recommended for food packaging, high quality stationery film, lamination films, textile packaging film, sealing layer in coextrusion.

Former trade name for this product was BorPure™.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 - 750 %550 - 750 %ISO 527-3
Tensile Modulus 0.350 - 0.450 GPa50.8 - 65.3 ksiMD/TD; ISO 527-3
Flexural Modulus 0.650 GPa94.3 ksiISO 178
Dart Drop, Total Energy 23.0 J
@Thickness 0.0500 mm
17.0 ft-lb
@Thickness 0.00197 in
1180 N; ISO 7765-2
Coefficient of Friction >= 0.50>= 0.50film to film; ISO 8295
Film Tensile Strength at Break, MD 30.0 - 50.0 MPa4350 - 7250 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 - 45.0 MPa3630 - 6530 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 138 - 142 °C280 - 288 °FDSC; ISO 3146
Vicat Softening Point 122 °C
@Load 1.02 kg
252 °F
@Load 2.25 lb
A50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 1.8 %<= 1.8 %ASTM D1003
Gloss >= 120 %>= 120 %20° of arc; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis RD204CF Polypropylene Random Copolymer
Borealis RE216CF Polypropylene Random Copolymer
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer
Borealis RD234CF Polypropylene Random Copolymer
Dow Bynel® 50E739 Anhydride Modified Polypropylene

PBOREA344 / 108604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.