Vulcanizates made from this compound exhibit a unique combination of characteristics. They are noted for their good flexibility, high transparency, and mechanical properties. The compounds are easily pigmented with ELASTOSIL® PT Pigment Pastes and have good processing characteristics. Application: ELASTOSIL® R 401/20 has many different uses, being suitable for molded articles and extrusions such as seals, sheet, tubing and profiles. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances. Information provided by Wacker Chemie AG. |