MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Crastin® HR5330HF NC010 PBT-IGF30
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Melt Density 1.29 g/cc
@Temperature 250 °C
0.0466 lb/in³
@Temperature 482 °F
Water Absorption 0.35 %
@Thickness 2.00 mm
0.35 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.150 %
@Thickness 2.00 mm
0.150 %
@Thickness 0.0787 in
Sim. to ISO 62
Viscosity Measurement 0.800.80Intrinsic viscosity; ISO 307, 1157, 1628
Viscosity Number 95 cm³/g0.95 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
 0.00050 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
0.00050 in/in
@Treatment Temp. 176 °F,
Time 48.0 hour
Postmolding shrinkage; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4, 2577
 0.0020 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
0.0020 in/in
@Treatment Temp. 176 °F,
Time 48.0 hour
Postmolding shrinkage; ISO 294-4
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 250 °C
10 g/10 min
@Load 4.76 lb,
Temperature 482 °F
8 cm³/10min Volumetric; ISO 1133
Spiral Flow 35.0 cm
@Pressure 80.0 MPa
13.8 in
@Pressure 11600 psi
width/thickness = 2mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psiISO 527-1/-2
Elongation at Break 3.2 %3.2 %ISO 527-1/-2
Tensile Modulus 8.50 GPa1230 ksiISO 527-1/-2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 7.50 GPa1090 ksiISO 178
Poissons Ratio 0.340.34
Shear Strength 55.0 MPa7980 psiASTM D 732
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.15 J/cm²
@Temperature -30.0 °C
5.47 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 62631-3-2
Dielectric Constant  4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.4
@Frequency 100 Hz
4.4
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 44.0 kV/mm1120 kV/inIEC 60243-1
 19.0 kV/mm
@Thickness 2.00 mm
483 kV/in
@Thickness 0.0787 in
Short Time; IEC 60243-1
 31.0 kV/mm
@Thickness 1.00 mm
787 kV/in
@Thickness 0.0394 in
Short Time; IEC 60243-1
Dissipation Factor  0.0025
@Frequency 100 Hz
0.0025
@Frequency 100 Hz
IEC 62631-2-1
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 450 V450 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
 15.0 µm/m-°C
@Temperature 55.0 - 160 °C
8.33 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
 25.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
13.9 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C83.3 µin/in-°FISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 145 µm/m-°C
@Temperature -40.0 - 23.0 °C
80.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Specific Heat Capacity 1.73 J/g-°C
@Temperature 250 °C
0.413 BTU/lb-°F
@Temperature 482 °F
Melt
Thermal Conductivity 0.280 W/m-K
@Temperature 250 °C
1.94 BTU-in/hr-ft²-°F
@Temperature 482 °F
Melt
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FISO 75-1/-2
Vicat Softening Point 215 °C419 °F50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 65.0 °C149 °F10°C/min; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 30.0 mm/min
@Thickness 1.00 mm
1.18 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 19 %19 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FOptimum, Injection
 240 - 260 °C464 - 500 °FRange, Injection
Mold Temperature 80.0 °C176 °FOptimum, Injection
 30.0 - 130 °C86.0 - 266 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %<= 0.040 %Injection
Hold Pressure >= 60.0 MPa>= 8700 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>PBT-IGF30<ISO 11469
PolymerPBT-I-GF30
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPBT-IGF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Crastin® SK605 NC010 PBT-GF30
Celanese Crastin® HR5330HFS NC010 PBT-IGF30
Celanese Crastin® LW9020 NC010 PBT+ASA-GF20
Celanese Crastin® LW9030 NC010 PBT+ASA-GF30
Celanese Crastin® CE15330 NC010 PBT-GF30FR(17)

PDSX5022 / 197662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.