MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and other thicknesses may be made available upon request. Adhesive seamed, heat shrinkable tubing and contour bottom heat shrinkable bags made from unsupported Mylar HS, and heat shrinkable heat sealed tubing and bags made from laminations of Mylar HS and a suitable sealant web, are used for packaging.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Average value for Mylar® films.
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm1.52 cc-mil/100 in²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/dayASTM E96 Procedure E
Oxygen Transmission 2.90 cc-mm/m²-24hr-atm7.37 cc-mil/100 in²-24hr-atmor 75 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 38.0 microns1.50 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882
Film Elongation at Break, TD 110 %110 %ASTM D882
Modulus of Elasticity 3.10 GPa450 ksi(stiffness), ASTM D882
Film Tensile Strength at Break, MD 214 MPa31000 psiASTM D882
Film Tensile Strength at Break, TD 234 MPa33900 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FMay be used to contain foods during baking above this temperature.
Shrinkage, MD 0.45 %
@Temperature 150 °C,
Time 1800 sec
0.45 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.
Shrinkage, TD 0.50 %
@Temperature 150 °C,
Time 1800 sec
0.50 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 150 Gauge
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 150 Gauge
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 150 Gauge
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 150 Gauge
DuPont Teijin Films Mylar® OB13AF Polyester Film, 150 Gauge

PDU675 / 33124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.