MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Performance Features: Manufactures of technical parts can achieve the highest levels of:
  • Wear and tear strength
  • Dimensional stability
  • Oil resistance
  • Low compression set
  • Dynamic load performance
  • Elasticity and flexibility
  • Temperature performance
  • Processing consistency

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage 0.030 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ASTM D2240
Hardness, Shore D 18ASTM D2240
Tensile Strength at Break 3700 psiASTM D412
Elongation at Break 900 %ASTM D412
100% Modulus 0.510 ksi
@Strain 100 %
ASTM D412
300% Modulus 0.800 ksi
@Strain 300 %
ASTM D412
Rebound 54 %Bayshore; ASTM D2632
Tear Strength 360 pliASTM D624
Abrasion 55mm3; ISO 34-1
Compression Set 43 %
@Temperature 22.8 °C,
Time 252000 sec
ASTM D395
 54 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 170 °CTMA Melt Range

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade

PHUQ120 / 159493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.