MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adflex Q 300F Thermoplastic Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin

Material Notes: Adflex Q 300 F is a thermoplastic polyolefin which has been developed for the extrusion or calendaring of soft film. Adflex Q 300 F can also be used as impact/toughened modifier of polypropylene homopolymer in extrusion applications. In strapping applications for instance, it notably decreases fibrillation and improves the process ability of the film at high drawing ratios. Adflex Q 300 F can be processed on any conventional PP extrusion line as well as on PVC calendars. It can also be blown on standard LDPE or LLDPE film lines. Applications: Agriculture Film, Bags & Pouches, Bottles For Consumer Goods, Bottles for Industrial Use, Collapsible Tubes, Film Wrap, Heavy Duty Packaging, Hygiene Film, Lamination Film, Peelable Film, Surface Protection Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³Method A; ISO 1183-1
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3636ISO 868
Tensile Strength at Break 13.0 MPa1890 psiISO 527-1,-2
Tensile Strength, Yield 9.00 MPa1310 psiISO 527-1,-2
Elongation at Break 550 %550 %ISO 527-1,-2
Elongation at Yield 35 %35 %ISO 527-1,-2
Flexural Modulus 0.330 GPa47.9 ksiISO 178
Charpy Impact, Notched  10.0 J/cm²
@Temperature -20.0 °C
47.6 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 10.0 J/cm²
@Temperature -40.0 °C
47.6 ft-lb/in²
@Temperature -40.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C122 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 78.0 °C172 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 95 %95 %ASTM D1003
Gloss 4.0 %
@Thickness 0.0500 mm
4.0 %
@Thickness 0.00197 in
@ 45°; ASTM D2457
 
Descriptive Properties
Processing MethodBlown Film; Extrusion Blow Molding; Sheet and Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LD 70013.BA Low Density Polyethylene Resin (European Grade)
ExxonMobil LD 22014.BA Low Density Polyethylene Resin (European Grade)
ExxonMobil LD 150013.BA Low Density Polyethylene Resin (European Grade)
LyondellBasell Petrothene NA202000 Low Density Polyethylene (LDPE), Wire/Cable Grade
LyondellBasell Lucalen A2920M Low Density Polyethylene

PEQT7009 / 218648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.