MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Polyolefin

Material Notes: Description

Invision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccISO 1183/1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8615 sec delay; ISO 868
Tensile Strength at Break 7.40 MPaISO 527
Tensile Stress at Strain 4.70 MPa
@Strain 100 %
ISO 527
Elongation at Break >= 350 %ISO 527
Tear Strength 45.0 kN/mISO 34/1
 
Descriptive Properties
Colorfastness/Weatherability 1240 Delta E (kJ/m^2)SAE J1885

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Celanese Celstran® PP-GF50-04 Black PP, 50% Glass Reinforced
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic

PASHU056 / 25020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.